1.Expressed as a m (w)/ m (c)(including gypsum),the CWD for complete hydration of a typical clinker ranges from approximately 0.37 to 0.62 as gypsum contents increase from 0 to 30%.
以水灰比m(w) /m (c)表示 (包含石膏中的水 ) ,当石膏质量分数由 0增至3 0 %时 ,典型矿物完全水化的化学需水量大约在 0 .3 7~ 0 .62之间 .收藏指正
2.Rare earth elements in a micro range of 4×10 -6 ~2×10 -4 can improve the burn ability of raw meal,reduce the free CaO and increase the alite content in cement clinker.
稀土元素在 4× 10 -6~ 2× 10 -4 的微量范围内可改善水泥生料易烧性 ,降低熟料中游离氧化钙 ,增加阿利特 (硅酸三钙 )含量。收藏指正