latex compound
3.TDI, PPG, HOA and DBT are put into a 4_mouth flask, stirred with nitrogen incoming, heated to 80-85℃ progressively, and reacted for 3h, followed by temperature decrease. The compound is added by solvent and neutralizer, stirred uniformly and emulsified by the addition of water, to obtain the PU latex after the solvent evaporation.

