1.When silicone rubber/metallic soapcontent was 10 PHR and glass fiber 5-10 PHR, the oxygen index of the ABS plastics was higher than 26, with less smoking, greater tensile strength, less decrease of impact strength better over-all properties.
2.Abstract: This paper is related to soap frost,that is inorganic content in soap and the organic acid acidifi-cation after saponification by oil and fat. NaOH≤0. 3% ,NaCl≤0. 2%,≥ SiO23% are suitable for soap base,be-cause of lower molecular acid and unsaturated acid in organic acid.
3.High solid content and stable soap-free emulsion of styrene (St) and butylacrylate (BA) was prepared in the presence of ionic hydrophilic monomer, nonionic hydrophilic macromolecule and amphiphilic monomer.