9.Abstract: Experiments indicated that under Tanggang material conditions and at the basicity range of 1.4~1.7, the sinter tumbler strength and reduction desintegration properties were worsen as Australian fine ores added ; but at the basicity range of 0.4~0.6,the sinter strength can improved with both adding of Indian fine ores or Australian fine ores.