6.2) For CRIC samples, nanocrystalline structure of thickness up to 2-3 um appeared in the remelted top surface layer, while the rapid recovery and recrystallization processes occurred in the heat affected zone (HAZ). Grains in the top layers were greatly refined with the formation of preferred orientation along (200) crystal plane.