1.a water blister
2.It was found that the sub-surface blister were prevented effectively by reducing Mg,Al,Ti contents in nodular cast iron (Mg<0. 055 %, Al<0. 03%,Ti<0. 03 % ), raising casting tempernture, dropping water content in mould sand, increasing venting quality and scattering NaF poweder in the mould surface
试验表明,采用减少球墨铸铁中残余的Mg、Al、Ti含量(Mg<0.055%、Al<0.03%、Ti<0.03%),提高浇注温度,降低型砂中含量,增大砂型透气性以及在砂型表面抖撒NaF粉等措施,能有效防止球墨铸铁件皮下气孔的产生。收藏指正